AZ150 ALUZINC STEEL COILS galvalume steel sheet is composed of aluminum-zinc alloy structure, which is composed of 55% aluminum, 43.5% zinc and 1.5% silicon solidified at a high temperature of 600°C. Its entire structure is composed of aluminum-iron-silicon-zinc, forming a dense quaternary crystal An alloy .The corrosion resistance of "aluminized zinc steel coil" is mainly due to the protective function of aluminum and aluminum. When zinc is worn, aluminum forms a dense layer of aluminum oxide, which prevents corrosion-resistant substances from further corroding the interior.
AZ120 ALUZINC STEEL COILS galvalume steel sheet is composed of aluminum-zinc alloy structure, which is composed of 55% aluminum, 43.5% zinc and 1.5% silicon solidified at a high temperature of 600°C. Its entire structure is composed of aluminum-iron-silicon-zinc, forming a dense quaternary crystal An alloy .The corrosion resistance of "aluminized zinc steel coil" is mainly due to the protective function of aluminum and aluminum. When zinc is worn, aluminum forms a dense layer of aluminum oxide, which prevents corrosion-resistant substances from further corroding the interior.
Fingerprint resistant GL steel sheet is an alloy coated steel sheet widely used in many fields such as building materials, home appliances, automobiles, environment, machinery, and ships. The galvanized steel sheet is covered with aluminum-zinc alloy on the surface of the steel sheet. RFP GL Coils is composed of 55% aluminum, 43.5% zinc and 1.5% silicon solidified at a high temperature of 600°C. The entire structure is composed of aluminum-iron-silicon-zinc, forming a dense An alloy-coated steel plate of quaternary crystal.
55% Alu GL COILS galvalume steel sheet is composed of aluminum-zinc alloy structure, which is composed of 55% aluminum, 43.5% zinc and 1.5% silicon solidified at a high temperature of 600°C. Its entire structure is composed of aluminum-iron-silicon-zinc, forming a dense quaternary crystal An alloy .The corrosion resistance of "aluminized zinc steel coil" is mainly due to the protective function of aluminum and aluminum. When zinc is worn, aluminum forms a dense layer of aluminum oxide, which prevents corrosion-resistant substances from further corroding the interior.